Form:
Subspherical powder
Preservation Condition:
Store tightly at room temperature and away from fire
Size:
D10: ≥10 μm
D50: 25-35 μm
D90: ≤53 μm
Custom particle size available
Density, g/cm3:
Apparent density: ≥4.4
Tap density: ≥5
Elements, wt.%:
Co: Bal
C: ≤0.35
Cr: 27.0-30.0
Mo: 5.0-7.0
Si: ≤1.0
Mn: ≤0.3
Fe: <0.75
O: <0.08
N: <0.15
H: <0.1
Ultimate Tensile Strength, MPa:
X&Y: 1090
Z: 1190
Tensile Strength, MPa:
X&Y, heat treatment: ≥1150
Z, heat treatment: ≥1070
Yield Strength, MPa:
X&Y, heat treatment: ≥660
Z, heat treatment: ≥615
Elongation, %:
X&Y, heat treatment: ≥21.0
Z, heat treatment: ≥23.0
Young's Modulus, GPa:
≥200
Linear Expansion Coefficient, *10-6/K:
14.1±0.5
Description:
CoCrMo material has excellent mechanical properties, wear resistance, corrosion resistance, biocompatibility and high specific strength. Typical applications for CoCrMo are orthopedic and dental implants, as well as gas turbine components.